YD-455 | 4 | 38-48 | | 1.6 | 用于需要高耐磨性但裂纹许可较少的部位 |
YD-480 | 5 | 40-50 | | 1.2~1.6 | 用于堆焊受磨损的中、低碳钢部件表面,如车轴、齿轮、搅拌叶片,行走主动轮等 |
YD-481 | 3 | 46-53 | | 1.2~1.6 | 用于堆焊工作温度低于450℃的轴及阀门等 |
YD-501 | 3 | 45-55 | 有裂纹 | 1.6 | 耐磨料磨损性能好,用于(洛阳中原,山西捷诚用过) |
YD-507 | 3 | 35-45 | | 1.6 | 用于堆焊工作温度低于450℃的轴及阀门等 |
YD-507Mo | 3 | 35-45 | | 1.6 | 用于堆焊工作温度低于510℃的轴及阀门等 |
YD-517 | 4 | 48-55 | | 1.6 | 用于堆焊轴及过热蒸汽阀件、搅拌机等 |
YD-537 | 4 | 48-55 | | 1.6 | 用于400℃温度下,受轻微腐蚀的磨损件,如橡胶密炼机辊 |
YD-556 | 2~4 | 55-61 | | 1.2~1.6 | 耐磨料磨损和耐金属间磨损性能较好,用于堆焊粮油机械叶轮、采煤机截齿、盾构机刀头、橡胶破碎辊/沟辊等 |
YD-557 | 2~5 | 55-61 | | 1.2~1.6 | 耐磨料磨损和耐金属间磨损性能较好,用于堆焊粮油机械叶轮、采煤机截齿、盾构机刀头、橡胶破碎辊/沟辊等 |
YD-575 | 3 | 55-61 | | 1.2~1.6 | 耐磨料磨损和耐金属间磨损性能较好,用于堆焊粮油机械,叶轮、采煤机截齿、盾构机刀头等 |
YD-582 | 3 | 55-62 | | 1.2~1.6 | 耐磨料磨损和耐金属间磨损性能较好,用于堆焊粮油机械,叶轮、采煤机截齿、盾构机刀头等 |
YD-5825 | 3 | 55-62 | | 1.2~1.6 | 耐磨料磨损和耐金属间磨损性能较好,用于堆焊粮油机械,叶轮、采煤机截齿、盾构机刀头等 |
YD-5826 | 3 | 55-62 | | 1.2~1.6 | 耐磨料磨损和耐金属间磨损性能较好,用于堆焊粮油机械,叶轮、采煤机截齿、盾构机刀头等 |
YD-5827 | 3 | 55-62 | | 1.2~1.6 | 耐磨料磨损和耐金属间磨损性能较好,用于堆焊粮油机械,叶轮、采煤机截齿、盾构机刀头等 |
YD-585 | 3~6 | 55-61 | | 1.2~1.6 | 耐磨料磨损和耐金属间磨损性能较好,用于堆焊粮油机械,叶轮、采煤机截齿、盾构机刀头、制砖机磨具等 |
YD-591 | 3 | 56-61 | 有裂纹 | 1.2~1.6 | 耐磨料磨损性能优良,用于耐磨衬板、采矿用齿等受磨料磨损的零件,可自保护焊接 |
HD-605 | 4~10 | 55-61 | 有裂纹 | 1.6 | 耐磨料磨损性能优良,用于耐磨衬板、水泥挤压辊、采煤机截齿、单齿辊等受磨料磨损的零件,可自保护焊接 |
YD-6055 | 4~10 | 55-61 | 有裂纹 | 1.6 | 耐磨料磨损性能优良,用于耐磨衬板、水泥挤压辊、采煤机截齿、单齿辊等受磨料磨损的零件,可自保护焊接 |
YD-6056 | 4~10 | 55-61 | 有裂纹 | 1.6 | 耐磨料磨损性能优良,用于耐磨衬板、水泥挤压辊、采煤机截齿、单齿辊等受磨料磨损的零件,可自保护焊接 |
YD-6057 | 4~10 | 55-61 | 有裂纹 | 1.6 | 耐磨料磨损性能优良,用于耐磨衬板、水泥挤压辊、采煤机截齿、单齿辊等受磨料磨损的零件,可自保护焊接 |
YD-621 | 2~4 | 55-68 | 有裂纹 | 1.6 | 耐磨料磨损性能优良,用于耐磨衬板、水泥挤压辊、采煤机截齿等受磨料磨损的零件,可自保护焊接 |